ABchimie 9111 UV Glue
Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others

Main features
- One-component
- Fast UV Curing
- Adhesion to many substrates
Product Description
ABChimie® 9111UV Glue is a soft, clear glue designed for the bonding of multiple substrates, including glass, metals, and plastics. Its viscosity allows for controlled application with high thicknesses (up to 4mm) without sagging. These qualities make ABChimmie 9111UV Glue ideal for small components with high-volume production, requiring adhesion between multiple substrates and optical transparency.
ABChimie 9111UV Glue is a urethane acrylate-based product with excellent adhesion to various substrates, including flexible materials such as plastics. It cures rapidly under UV light, has zero VOCs, and can be applied to high-speed manufacturing processes to increase productivity. ABChimmie 9111UV Glue is in full compliance with REACH and RoHS regulations.
Product Key Features
- Transparent urethane acrylate glue
- No yellowing
- Allows for thick, controlled application
- Fast UV cure (mercury lamp) for high-speed processing
- Solvent-free formulation (no VOCs)
Applications
- Components requiring optical transparency ex. glass, lenses.
- Adhesion to various substrates, ex. metal to glass, metal to plastic, glass to plastic, etc.
- Rework or repair.
- Can be used to seal plastic casings on PCBs.
- Printed circuit assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Additional Information
Frequently Asked Questions About ABChimie® 9111 UV
What are typical applications for ABChimie® 9111 UV?
ABChimie® 9111 UV is a UV-curable glue designed for the bonding and protection of printed circuit board assemblies (PCBs) and electronic components in demanding manufacturing environments, including:
-
Automotive electronics (e.g., control units, sensors)
-
Industrial automation (e.g., motor drives, PLCs)
-
Consumer electronics (e.g., smart devices, wearables)
-
Other high-reliability electronic assemblies
What is the shelf life of ABChimie® 9111 UV?
ABChimie® 9111 UV has a shelf life of 12 months when stored at 5–30°C in tightly sealed, opaque containers. The product must be sealed away from excessive heat (>40°C). Before use, allow the product to equilibrate for 24 hours at 18–32°C for optimal performance. Due to settling, glue should be mixed before use.
What is the recommended curing method for ABChimie® 9111 UV?
ABChimie® 9111 UV is UV-curable and should be cured with a mercury lamp. The minimum UVA dose is 500 mJ/cm² for a 100 μm thickness. The LED-curable version is ABChimie® 9111 UV LED. Higher UVA doses do not negatively affect final properties.
Learn More About ABChimie® 9111 UV
ABChimie® 9111 UV is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This UV-curable resin delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for applications in automotive electronics, industrial automation, consumer electronics, and other high-reliability assemblies.
Main Advantages of ABChimie 9111 UV
ABChimie® 9111 UV cures rapidly under UV light, enabling integration into both batch and inline production. The resin forms a durable, high-performance layer that protects assemblies while supporting high-throughput manufacturing.
ABChimie® 9111 UV provides excellent mechanical protection. The hardness helps resist scratches, abrasion, and minor impacts, ensuring long-term stability of encapsulated components.
ABChimie® 9111 UV is thixotropic: it maintains a stable, non-running consistency at rest but flows easily under shear during application. This ensures precise placement, minimal sagging, and uniform coverage before rapid UV curing.
ABChimie® 9111 UV bonds strongly to flexible substrates, including plastics and polymer-based PCBs. Its adhesion ensures reliable protection even on surfaces that bend or flex, ideal for wearables, flexible electronics, and lightweight assemblies.
How to Choose a Resin
Selecting the most suitable resin requires consideration of key factors:
- ✔ Norms & Compliance
- ✔ Environment / Exposure Conditions
- ✔ Repairability
- ✔ Electrical Performance
- ✔ Application Method
- ✔ Operating Temperature
Compliance You Can Trust ✅
ABChimie® 9111 UV meets stringent industry standards, ensuring reliability and regulatory adherence for OEMs and contract manufacturers:
- REACH Compliant
- RoHS 2011/65/EU Compliant
Curing Tip: ABChimie 9111 UV cures with UV rays. It is crucial to use the appropriate equipment, as well as the recommended settings, to achieve the best properties of the resin.
Emission Spectrum of Mercury Lamp
Ref. Leistung / ref power ln % over wavelength in nm
Key Curing Properties
Mercury
200-400 nm
100 mJ/cm2 for 100 μm thickness, 600 mJ/cm2 for 1000 μm thickness
Varies
Typical property values shown for reference only and should not be used as specifications.
Alternative to Mercury Lamp Curing of ABChimie 9111 UV
ABChimie 9111 UV is also available in the LED - version, which cures by LED Lamp.
ABChimie 9111 UV LED [Go to 9111 UV LED Product Page↗]
- Thixotropic resin
- Fluorescent under UV light
- Excellent adhesion to flexible substrates
- Immediate curing with UV LED exposure
Best suited for: High-speed process looking to use LED light for curing