ABchimie836UV LED Soft Dual Cure Conformal Coating

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ABchimie836UV LED Soft Dual Cure Conformal Coating

Main features

  • One Component
  • Dual Cure (UV LED and Humidity)
  • Excellent Moisture Resistance

Product Description

ABChimie® 836UV LED is a transparent urethane acrylate conformal coating designed to provide mechanical and environmental protection to electronic components and assemblies. It features dual-cure technology (UV and humidity), which allows for the complete crosslinking through the entire PCB, even in areas that may be covered by shadow. The coating also allows the PCB to be soldered through without producing toxic gases.

ABChimie 836UV LED exhibits excellent moisture resistance in humid environments (Log Ohm> 10.5, IPC CC 830, SIR per IPC TM 650 2.6.3.4), which makes it ideal for conformal coating applications. The ideal application method is selective coating.  One of its advantages is that it cures rapidly under UV light, has zero VOCs, and can be applied to high-speed manufacturing processes to increase productivity. ABChimmie 836UV LED is in full compliance with REACH and RoHS regulations, and also has UL94 V0 and UL746E (QMJU2-E308681) certifications.

Product Key Features

  • Transparent 
  • Dual Cure (UV + Humidity)
  • Thin film thickness (30 - 130 microns)
  • Excellent adhesion to PCBs 
  • Resists mold growtn
  • Fast UV cure for high volume production
  • Solvent-free formulation (no VOCs)
  • Spray and Selective Coating (ideal) applications 
  • UL94 V0 and UL746e

Applications

  • Conformal coating for Printed circuit assemblies. 
  • Protection for plastic casings or covers.
  • Protection for optically clear applications ex. lenses. 
Product Family

ABCHIMIE 836UVLED

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Transparent liquid
Film ThicknessFilm Thickness
30 - 130 µm
Electrical Properties
Breakdown VoltageBreakdown Voltage
1500 V
Thermal Properties
Coefficient of Thermal Expansion (CTE), α1Coefficient of Thermal Expansion (CTE), α1
66 ppm/°C
Coefficient of Thermal Expansion (CTE), α2Coefficient of Thermal Expansion (CTE), α2
193 ppm/°C
Glass Transition Temperature (Tg)Glass Transition Temperature (Tg)
35 °C
Operating TemperatureOperating Temperature
-50 - +150 °C
UL 94 RatingUL 94 Rating
V-0
Physical Properties
ViscosityViscosity
52.5 mPa.s

Additional Information

Frequently Asked Questions About ABChimie® 836 UV LED

What are typical applications for ABChimie® 836 UV LED?

ABChimie® 836 UV LED is a UV-curable conformal coating designed to protect printed circuit board assemblies (PCBs) and components in demanding manufacturing environments, including:

  • Automotive electronics (e.g., control units, sensors)
  • Industrial automation (e.g., motor drives, PLCs)
  • Consumer electronics (e.g., smart devices, wearables)
  • Other high-reliability electronic assemblies

Why choose ABChimie® 836 UV LED?

ABChimie® 836 UV LED delivers rapid UV curing, excellent electrical insulation, optical transparency, and strong adhesion to flexible substrates. It supports high-throughput manufacturing while providing durable protection for sensitive components.

What is the shelf life of ABChimie® 836 UV LED?

ABChimie® 836 UV LED has a shelf life of 12 months when stored at 5–30°C in tightly sealed containers. Prior to use, allow the product to equilibrate for 24 hours at 18–32°C for optimal performance.

What happens after the shelf life?

Using ABChimie® 836 UV LED past its shelf life may alter viscosity, affecting uniformity and application performance. Always use an in-date product for reliable results.

What is the recommended thickness for ABChimie® 836 UV LED?

ABChimie® 836 UV LED coating thickness depends on the application method.

Recommended thickness 30–130 microns
Spraying: 30–90 microns
Selective coating machine (film coater): 90–130 microns (380mm/s)

What safety precautions should I take?

Use ABChimie® 836 UV LED in a well-ventilated area, avoid skin and eye contact, and follow all Safety Data Sheet (SDS) guidelines. Keep away from open flames and sparks.

Can I adjust the viscosity?

ABChimie® 836 UV LED can be customized for variable viscosities. Contact our team for guidance.

Should I control the application environment?

ABChimie® 836 UV LED should be applied at a minimum temperature of 16°C and a minimum relative humidity of 50%. The relative humidity of at least 50% is recommended for the secondary polymerization. Before applying, the PCB must be clean, dry, and free of moisture. A stage in an oven at 80°C for 4 hours is usually sufficient.

Learn More About ABChimie® 836 UV LED

ABChimie® 836 UV LED is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This UV-curable conformal coating delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for automotive, industrial, consumer, and high-reliability assemblies.

Main Advantages of ABChimie 836 UV LED

dual cure technology

ABChimie® 836 UV LED cures through a dual mechanism: UV exposure initiates rapid surface curing, while moisture ensures complete curing throughout the coating.

mechanical protection

Provides excellent mechanical protection, resisting scratches, abrasion, and minor impacts to ensure long-term component stability.

ability to solder

Can be soldered through without generating highly toxic gases, maintaining coating integrity.

excellent adhesion in harsh environments

Provides strong adhesion in harsh conditions, resisting moisture, chemicals, and temperature changes.


How to Choose a Conformal Coating

  • ✔ Norms & Compliance
  • ✔ Environment / Exposure Conditions
  • ✔ Repairability
  • ✔ Electrical Performance
  • ✔ Application Method
  • ✔ Operating Temperature

Compliance You Can Trust ✅

  • REACH Compliant
  • RoHS 2011/65/EU Compliant
    UL94 V0
    UL746E (QMJU2-E308681)

Curing Tip: ABChimie 836 UV LED cures with UV rays. Use the recommended equipment and settings to achieve optimal properties.

Ref. Leistung / ref power ln % over wavelength in nm

PTM6000HV-SP thermal impedance versus bondline thickness

Key Curing Properties

Lamp Type
LED
Emission Spectrum of LED
395 nm
Minimum UVA Dose
3000 mJ/cm2
Coating Thickness
100 μm
Minimum UVA Power
500 mW/cm2

Typical property values shown for reference only and should not be used as specifications.

Application tips

How to Optimise for the Best Results

 
PCB Preparation

PCBs must be completely dry and thoroughly clean, with no dust, grease, wax, or other contaminants. All flux residues must be removed to prevent corrosion or malfunctions.

How to clean the PCB

For cleaning equipment or removing uncured ABChimie836UV or UV LED varnish, use SND or ABclean solvent.

UV Recommendation

Use the correct UV equipment and recommended settings to achieve optimal properties. UV exposure plus moisture curing ensures complete polymerization.

Curing Mechanism

Curing Mechanism: UV light creates the first cure; moisture completes the curing process over 7 days.

Double-Curing Mechanism

How does Moisture Cure Work?

Exposure to UV light activates photoinitiators, triggering rapid polymerization for surface cure. A secondary moisture-activated cure completes the process in shadowed areas over 7 days at ≥50% RH.

ABChimie 836 UV LED is also available in the mercury lamp version, which cures with a mercury lamp.

ABChimie 836 UV [Go to 836 UV Product Page↗]

  • Conformal Coating
  • Fluorescent under UV light
  • Excellent adhesion to flexible substrates
  • Dual curing with UV light exposure and moisture curing

Best suited for: High-speed process using LED light for curing

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers