3M EC-3587

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M EC-3587

Main features

  • Structural Bonding And Fairing
  • Selectable Assembly Work Life
  • Sandable Non Sag Gap Filling

Product Description

3M Scotch-Weld Structural Adhesive EC-3587 B/A Gray is a gray, two-part polyurethane structural adhesive available in B-1/4 and B-1 work-life classes. It cures at room temperature or with heat to a tough, impact-resistant material that bonds many prepared metal and plastic substrates. The non-sag mixture also functions as a void filler or fairing compound and can be sanded after cure. Class B-1/4 provides 5 to 20 minutes of work life, while Class B-1 provides 40 to 150 minutes at 23 deg C for different part sizes and placement windows.

Key features

  • Structural Bonding And Fairing: One material can bond, fill gaps, and form a sandable fairing surface.
  • Selectable Work Life Classes: B-1/4 and B-1 versions provide different application windows.
  • Tough Non Sag Urethane: The mixed adhesive holds its shape and cures to an impact-resistant material.

Applications

Structural bonding of prepared metals and plastics, void filling, gap filling, and sandable fairing work.

Product Family

3M EC-3587

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Processing values are separated by B-1/4 and B-1 class where they differ.

PropertyValueUnitMethod / condition
Available classesB-1/4; B-1-Select before processing
Solids100%Both components and both classes
Mix ratio by weight100:100B:ABoth classes
Mix ratio by volume175:100B:ABoth classes
B-1/4 work life5 to 20min100 g mixed at 23 deg C
B-1 work life40 to 150min100 g mixed at 23 deg C
Mixed flow0.1inMIL-S-8802 Figure 1
Technical properties

After-processing / final-state properties

Cured overlap-shear results remain separated by B-1/4 and B-1 class.

PropertyValueUnitMethod / condition
Hardness62Shore DCured; both classes
B-1/4 overlap shear3390psiFPL-etched aluminum; tested at -40 deg C
B-1 overlap shear3765psiFPL-etched aluminum; tested at -40 deg C
B-1/4 overlap shear2450psiFPL-etched aluminum; tested at 24 deg C
B-1 overlap shear2512psiFPL-etched aluminum; tested at 24 deg C
B-1/4 overlap shear476psiFPL-etched aluminum; tested at 82 deg C
B-1 overlap shear475psiFPL-etched aluminum; tested at 82 deg C

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers