3M 8672
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

Main features
- UV-Resistant Outdoor Surface Protection
- 8-Mil Conformable Erosion Barrier
- High-Peel Acrylic Surface Adhesion
Product Description
3M Polyurethane Protective Tape 8672 is an 8 mil outdoor-grade polyurethane tape with acrylic pressure-sensitive adhesive and a polyester liner for leading-edge erosion and abrasion protection. The 6 mil polyurethane film is formulated for ultraviolet resistance and resists puncture, tearing, abrasion, and erosion, while the thin construction conforms over curved surfaces. The tape can be painted or applied over painted surfaces, and its acrylic adhesive provides high peel strength on tested aluminum, acrylic enamel, and ABS surfaces. It is designed for aircraft production and maintenance and other aerospace or industrial surfaces exposed to outdoor wear, including rain and sand erosion.
Key features
- UV-resistant outdoor polyurethane: The protective film is formulated for ultraviolet exposure and resists puncture, tearing, abrasion, and erosion in outdoor service.
- Thin conformable construction: The 8 mil total tape thickness follows curved surfaces while providing a durable leading-edge protective layer.
- High-peel acrylic adhesion: The acrylic adhesive provides measured peel adhesion on bare aluminum, acrylic enamel, and ABS while retaining a pressure-sensitive format.
Applications
Use 3M Polyurethane Protective Tape 8672 for leading-edge, erosion, scratch, and abrasion protection on aerospace and industrial surfaces, including painted or curved areas.
TDS, SDS & Technical Documents
Technical Specifications
Mechanical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Film material | Polyurethane | Outdoor-grade protective film | |
| Film thickness | 0.006 | in | 0.15 mm |
| Adhesive | Acrylic pressure-sensitive adhesive | Product construction | |
| Adhesive thickness | 0.002 | in | 0.06 mm |
| Liner | Polyester | Easy-release liner | |
| Tensile strength at break | 40 | lb/in | Typical; 700 N/100 mm; ASTM D882 |
| Elongation at break | 500 | % | Typical; ASTM D882 |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Approximate applied thickness | 0.008 | in | 0.21 mm; film plus adhesive; liner excluded |
| Peel adhesion to bare aluminum | 60 | oz/in | Typical; 66 N/100 mm; ASTM D1000 at 21 deg C |
| Peel adhesion to acrylic enamel | 43 | oz/in | Typical; 48 N/100 mm; ASTM D1000 at 21 deg C |
| Peel adhesion to ABS plastic | 50 | oz/in | Typical; 55 N/100 mm; ASTM D1000 at 21 deg C |
| Maximum service temperature | 180 | deg F | 82 deg C |