3M 760 UV

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 760 UV

Main features

  • High-Modulus, High Shore-a Hardness Formulation
  • Moisture-Cure Sealing Processing
  • Isocyanate-Free, Low VOC Formulation

Product Description

3M™ SMP Adhesive Sealant 760UV is a one-component, moisture-curing Silane Modified Polymer (SMP) sealant that forms a permanent, elastic bond. Designed as an isocyanate-free alternative to traditional polyurethanes, it features excellent UV resistance and high tensile strength capable of replacing mechanical fasteners. This high-modulus, high Shore-A hardness paste effectively bonds to a wide array of materials, including plastics, metals, fiberglass, and wood.

Key features

  • Isocyanate-free performance: One-component, low VOC formulation cures with moisture and can be painted when wet.
  • High-strength bonding: High modulus and high Shore-A hardness formulation delivers strong, permanent elastic bonds that can replace rivets and mechanical fasteners.
  • Environmental durability: Provides excellent resistance to UV, water, and salt spray.

Applications / Suitable for

  • Bonding floors, exterior/interior panels, and roofs for trucks, trains, trailers, and vans
  • General industrial and construction applications
  • Bonding dissimilar materials like plastics, metals, fiberglass, and wood
Product Family

3M 760 UV

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
SolidsSolids
100 %
Specific GravitySpecific Gravity
1.61
Physical Properties
Tack-Free TimeTack-Free Time
10-30 minutes
ViscosityViscosity
Thick paste mPa.s
VOCVOC
13 g/l
Mechanical Properties
ElongationElongation
>100 %

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Specific Gravity 1.61 - -
Consistency Thick Paste - -
VOC Content 13 g/L -
Tack-Free Time 10-30 minutes at 73°F and 50% Relative Humidity
Rate of Cure > 1/8 (3.5 mm) inches per 24 hour at 73°F and 50% RH
Approximate Coverage 126 lineal feet 10.5 oz. cartridge, 1/8" (3 mm) bead
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Shore A Hardness 55 - ASTM C661
Tensile Strength 260 psi (1.8 MPa) ASTM D412
Elongation at Break > 100 % ASTM D412
100% Modulus > 145 psi (> 1 MPa) ASTM D412
Service Temperature -40 to 212 °F (-40°C to 100°C)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers