3M 30NF
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

Main features
- Water-Dispersed Contact Adhesive
- Heat-Resistant Laminate Bonding
- Greenguard-Certified Wood and Laminate Bonding
Product Description
3M™ Fastbond™ Contact Adhesive 30-NF is a water-dispersed, sprayable polychloroprene contact adhesive offering a remarkably long bonding range and high coverage. Non-flammable in the wet state, it is engineered to create post-formable, heat-resistant bonds for demanding assembly tasks. This GREENGUARD-certified formulation effectively bonds most foamed plastics, plastic laminate, wood, plywood, and canvas to themselves and to each other.
Key features
- Water-dispersed formula: Non-flammable in the wet state, improving workplace safety while providing high surface coverage.
- High performance: Post-formable and highly heat resistant, making it exceptionally effective for decorative laminates and millwork.
- Low emissions: GREENGUARD certified for low chemical emissions, addressing or contributing to multiple LEED EQ credits.
Applications / Suitable for
- Bonding foamed plastics, plastic laminate, wood, plywood, and canvas
- Use with swinging type fire doors of hollow metal and steel composite types
- Interior building materials requiring low chemical emissions
Technical Specifications
General Properties
Thermal Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Base | Polychloroprene | - | - |
| Color | Green (Wet) / Dark Green (Dry) | - | Also available in Neutral formulation |
| Solids Content by Weight | 47 - 51 | % | - |
| Net Weight | 8.9 - 9.3 | lb/gal | (1.06 - 1.11 kg/L) |
| Viscosity | 200 - 750 | cP | at 27°C (80°F) |
| Coverage | 680 | ft²/gal | at 3 g/ft² dry |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180° Peel Adhesion | 560 | oz/in | Canvas to Steel, 72 h at 23°C (73°F) |
| Overlap Shear Strength | 480 | lb/in² | Birch to Birch at 23°C (73°F) |
| Overlap Shear Strength | 60 | lb/in² | Birch to Birch at 82°C (180°F) |
| Flatwise Tensile Strength | 113 | lb/in² | High pressure laminate to particle board at 23°C (73°F) |