3M 1357

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 1357

Main features

  • High Initial Contact Strength
  • High Heat Resistance
  • Up to 30-Minute Bonding Window

Product Description

3M™ Neoprene High Performance Contact Adhesive 1357 is a versatile polychloroprene-based contact adhesive that delivers excellent initial strength and high heat resistance. It is designed to bond a wide variety of substrates including rubber, cloth, metal, wood, foamed glass, paper honeycomb, and decorative plastic laminates. This high-performance adhesive features a long bonding range of approximately 30 minutes, providing ample open time for positioning and complex assembly.

Key features

  • High heat resistance: Maintains strong, durable bonds even under demanding thermal conditions.
  • Excellent initial strength: Delivers immediate holding power upon contact to streamline assembly processes and allow for immediate machining.
  • Long bonding range: Offers approximately 30 minutes of open time, allowing flexibility during application and part positioning.

Applications / Suitable for

  • Bonding rubber, cloth, and metal
  • Assembling wood and wood veneers
  • Adhering foamed glass, paper honeycomb, and decorative plastic laminates
Product Family

3M 1357

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
AppearanceAppearance
Gray/Green, Light Yellow
SolidsSolids
23 — 27 %
Thermal Properties
Flash PointFlash Point
-26 °C
Mechanical Properties
Peel StrengthPeel Strength
28 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Polychloroprene - -
Color Gray/Green, Light Yellow - -
Solids Content by Weight 23-27 % -
Viscosity 200-450 cP at 27°C (80°F)
Flash Point -26 °C TCC
Bonding Range Approx. 30 minutes at 21°C (70°F) and 35% R.H.
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications[cite: 8].

Property Value Unit Method / condition
180° Peel Adhesion 54 N/cm Canvas to Steel, 72 h at 23°C (73°F)
Overlap Shear Strength 3.1 MPa Birch to Birch, 2 week cure at 23°C (73°F)
Overlap Shear Strength 6.6 MPa Birch to Birch, 3 week cure, tested at -34°C (-30°F)

Leading Brands Trust in Our Products and Services

  • Jabil
  • Linxens
  • Magna
  • Medtronic
  • NXP
  • Philips
  • Semikron
  • Teledyne
  • Thales
  • Vishay
  • ZF
  • AMS
  • Apple
  • Audi
  • Broadcom
  • Borgwarner
  • Bosch
  • Eaton
  • Henkel
  • Honeywell
  • Hysol
  • Intel
Products that Perform|Knowledge that Serves|Service that Delivers